Test item 测试名称:Polymer Materials Electrical Performance Test 高分子材料电学性能测试
Test info 测试内容:
Test Item | Test Standard | Test Condition and Applied Range | Test Period | Sample Requirement | Note |
绝缘材料表面电阻率 | ASTM D 257 | 测量范围: | 7 working days | 片材,100mm边长的正方形或100mm直径的圆, 3pcs. |
|
IEC 60093 | |||||
GB/T 1410 | |||||
GB/T 1692(硫化橡胶) | |||||
绝缘材料体积电阻率 | ASTM D 257 | 测量范围: | 7 working days | ||
IEC 60093 | |||||
GB/T 1410 | |||||
GB/T 1692 (硫化橡胶) | |||||
防静电材料表面电阻率 | ANSI/ESD S11.11 | 测量范围: | 7 working days | 最小面积尺寸 |
|
介电强度 | ASTM D 149 | 测量电压范围:0~50000V | 7 working days | 视使用的电极尺寸而定,一般要求片材,100mm边长的正方形或100mm直径的圆,厚度在1-2mm,5pcs. |
|
IEC 60243-1 | |||||
GB/T 1408.1 | |||||
GB/T 1695 | |||||
介电击穿电压 | ASTM D 149 | 测量电压范围:0~50000V | 7 working days | 视使用的电极尺寸而定,一般要求片材,100mm边长的正方形或100mm直径的圆,厚度在1-2mm, 5pcs. |
|
IEC 60243-1 | |||||
GB/T 1408.1 | |||||
GB/T 1695 | |||||
耐电压 | ASTM D 149 | 电压测量范围:0~50000V 须指定测试电压值 | 7 working days | 视使用的电极尺寸而定,一般要求片材,100mm边长的正方形或100mm直径的圆,厚度在1-2mm,5pcs. |
|
IEC 60243-1 | |||||
GB/T 1408.1 | |||||
GB/T 1695 | |||||
静电衰减时间 | 客户提供 | 测试电压范围:±1000V | 7 working days | 片状样品 | 默认测试环境条件23℃, 50%RH. |
摩擦电压 | 客户提供 | 测试电压范围:±2000V | 7 working days | 产品 | 默认测试环境条件23℃, 50%RH. |